To avoid the fracture of the reinforced all-resin carbon strip in the printing process, you can start from the following aspects:
First, choose the right carbon belt and paper
1.Carbon strip quality: Ensure the use of high-quality reinforced all-resin carbon strips, the base film should have a certain strength and thickness, can withstand the tension during the printing process without breaking.
2.Paper matching: Choose paper that matches the carbon strip and avoid using paper with a surface that is too smooth or rough, which may cause the carbon strip to not be in close contact with the paper, increasing the risk of breakage.
Second, adjust the printer Settings
1.Tension adjustment: Check and adjust the carbon tape tension Settings in the printer to ensure that the tension is even and moderate. Too much tension may cause the carbon strip to overstretch and break, and too little tension may affect the print quality.
2.Temperature and speed: According to the characteristics of carbon belt and paper, set the printing temperature and speed of the printer reasonably. Too high a temperature may cause the carbon strip to melt and break, while too fast a speed may affect the bonding effect between the carbon strip and the paper.
3.Print concentration: Adjust the print concentration to the lowest concentration that can clearly print, to avoid too high a concentration that causes the carbon belt to be broken by too much heat and pressure during the printing process.
Third, the correct loading and use of carbon belt
1.Correct loading: Follow the instructions in the printer's manual to properly load the carbon strip and ensure it is placed flat. Avoid carbon tape curling or improper winding resulting in breakage during printing.
2.Avoid overuse: pay attention to the service life of the carbon belt, and replace the aging carbon belt in time. Aging carbon belt material may become brittle and prone to fracture during the printing process.
Fourth, regular maintenance and cleaning
1.Clean the print head: Clean the print head and carbon strip sensor regularly to remove dust and dirt. These impurities may affect the smooth passage of the carbon belt and increase the risk of fracture.
2.Check the printer parts: Regularly check the printer roller, tension wheel and other parts are damaged or need to be replaced. Damaged parts can cause the carbon strip to break under uneven tension during printing.
Fifth, pay attention to environmental factors
1.Temperature and humidity: Keep the temperature and humidity of the printing environment within the appropriate range. Too high or too low temperature, as well as humidity, can affect the performance of the carbon belt and increase the risk of fracture.
2.Avoid pollution: Ensure that the printing environment is clean and dust-free, and avoid the carbon belt being polluted and affecting its printing effect and durability.
In summary, by choosing the right carbon tape and paper, adjusting the printer Settings, correctly loading and using the carbon tape, regular maintenance and cleaning, and paying attention to environmental factors, the problem of fracture in the printing process of reinforced all-resin carbon tape can be effectively avoided.